Air-blast loading is a serious threat to military and civil vehicles, buildings, containers, and cargo. Applications of sandwich-structured composites have attracted increasing interest in modern lightweight design and in the construction of dynamic loading regimes due to their high resistance against blast and ballistic impacts. The functional properties of such composites are determined by the interplay of their face sheet material and the employed core topology. The core topology is the most important parameter affecting the structural behavior of sandwich composites. Therefore, this contribution presents a thorough numerical investigation of different core topologies in sandwich-structured composites subjected to blast loading. Special emphasis is put on prismatic and lattice core topologies displaying auxetic and classical non-auxetic deformation characteristics in order to illustrate the beneficial properties of auxetic core topologies. Their dynamic responses, elastic and plastic deformations, failure mechanisms, and energy absorption capabilities are numerically analyzed and compared. The numerical studies are performed by means of the commercial finite element code ABAQUS/Explicit, including a model for structural failure.
Abstract
Two types (with and without a hydrolysis stabilizer) of polyamide 6.6 (PA6.6) reinforced with 30% w/w glass fibres were examined against the influence of automotive cooling fluids, e.g. ethylene glycol aqueous solutions. The overall goal was to find a methodology to compare the performance of PA6.6 materials against the impacts of the hydrolysis environment. The stabilizer effect on the hydrolytic resistance of the materials was assessed using tensile tests according to ISO 527, and their strain‐at‐break values were evaluated in more detail. The degradation mechanism of both PA types was monitored by infrared spectroscopy and SEM. The material lifetime was described by the Arrhenius equation. The results show that the hydrolysis stabilizer operates effectively at low temperature but exhibits weak performance above 130 °C, which is explained by faster consumption of the stabilizing agent. © 2021 The Authors. Polymer International published by John Wiley & Sons Ltd on behalf of Society of Industrial Chemistry.